560 products match
![]() |
EP42HT-2ANLV Thermally conductive/electrically insulative. Serviceable from -100°F to +350°F. Chemically resistant to water, oils, fuels, acids, bases. Dimensionally stable. Good flow. |
![]() |
EP42HT-2AO Thermally conductive, electrically insulative. Ideal for potting and encapsulation. Castable up to 3-4 inches. Excellent chemical resistance. Enhanced thermal cycling capabilities. Good flow. Serviceable from -100°F to +400°F. Impervious to intermittent exposures to steam. Shore D hardnes >80. |
![]() |
EP42HT-2AO-1 Black Good heat conduction. Serviceable from 4K to +400°F. Resists water, oils, fuels. Excellent dielectric properties. Enhanced dimensional stability. Castable up to 2-3 inches thick. Low shrinkage upon cure. Good flow. Meets NASA low outgassing standards. |
![]() |
EP42HT-2FG Black Food grade epoxy system certified to meet FDA CFR 175.105. Excellent resistance to fats, oils, acids, alkalis and many solvents. Withstands boiling water, radiation, chemicals, steam and frozen storage conditions. Strong bonds to similar/dissimilar substrates. Service temperature range -60°F to +450°F. Black in color. |
![]() |
EP42HT-2FG Food grade epoxy system toxicologically evaluated to meet the NSF/ANSI 51.4.1 (2009) standard for food equipment materials. Certified to meet FDA CFR 175.300. Excellent resistance to fats, oils, acids, alkalis and many solvents. Withstands boiling water, radiation, chemicals, steam and frozen storage conditions. Strong bonds to similar/dissimilar substrates. Service temperature range -60°F to +450°F. Low viscosity. |
![]() |
EP42HT-2HV1 Chemical resistant, two component, room temperature curable epoxy. Serviceability from -60°F to +450°F. Withstands exposure acids, alkalis, solvents, sterilants such as radiation, steam, EtO. Post curing is recommended to optimize properties. Castable to thicknesses exceeding 2-3 inches. |
![]() |
EP42HT-2LO NASA low outgassing approved epoxy for service from -60°F to 450°F. Cures at ambient temperatures. Tensile strength >12,000 psi. Shore D hardness 80-90. Superior dimensional stability. Remarkable chemical resistance. Withstands 1,000 hours 85°C/85% RH. Castable in thicknesses exceeding 2-3 inches. Vacuum compatible. |
![]() |
EP42HT-2LTE Ultra low coefficient of thermal expansion. Two component, room temperature curing epoxy. Reliable electrical insulator. Unsurpassed dimensional stability. Low linear and volumetric shrinkage upon cure. Serviceable from -60°F to +300°F. Withstands 1,000 hours 85°C/85% RH. |
![]() |
EP42HT-2Med Black USP Class VI approved. Serviceable from -60°F to 450°F. Withstands multiple cycles of medical sterilization including radiation, EtO, autoclaving and chemical sterilants. Shore D hardnes >75. Used for bonding, sealing, coating, casting. Can be cured up to 2-3 inches thick. Cures at ambient temperature or more quickly at elevated temperatures. |
![]() |
EP42HT-2Med Low viscosity, two part epoxy with outstanding chemical resistance. Passes USP Class VI biocompatibility tests. Capable of withstanding repeated sterilization cycles including radiation, EtO, chemical sterilants, autoclaving. Serviceable from -60°F to +450°F. Cures at room or elevated temperatures. Available in amber-clear and black colors. Castable in thicknesses up to 2-3 inches. |